模具逃氣系統
Mold air venting system
在塑料射出成型與金屬壓鑄中「逃氣」是極為關鍵的設計。當熔融塑料或金屬高壓充填入模具型腔時,必須將型腔內的空氣以及高溫塑料產生的揮發氣體/裂解氣迅速排出。如果逃氣不良,會導致:
- 焦痕:氣體被絕熱壓縮產生極高溫,燒焦塑料尾端。
- 短射:殘留氣體阻擋流道,導致產品缺料。
- 結合線強度不足:氣體積在兩股料流匯合處,導致結合線明顯且易斷裂。
- 表面氣泡 / 氣孔
In plastic injection molding and die casting, venting is a critical design consideration. When molten plastic or metal is injected into the mold cavity under high pressure, the air inside the cavity—along with volatile gases and thermal degradation byproducts generated by high-temperature plastics—must be rapidly expelled. Poor venting leads to several severe defects:
- Burn Marks (Diesel Effect): Gases are adiabatically compressed to extremely high temperatures, burning the trailing edge of the plastic.
- Short Shot: Trapped gases obstruct the flow path, causing incomplete mold filling.
- Weak Weld Lines: Gas gets trapped at the convergence of two melt fronts, making weld lines prominent and prone to fracture.
- Surface Voids / Gas Bubbles